Blister tray packaging

   The reason for the uneven wall thickness of the tray blister packaging is that the unreasonable design leads to the uneven wall thickness of the part of the tray blister packaging during the processing. In our normal production process, due to the dead Angle of product design, the force in the material processing process is uneven, which makes the wall thickness uneven. Therefore, in the design process of tray blister packaging, I should also pay attention to the structure of tray blister packaging to be reasonable.

   Reason 1: The heating temperature of the tray blister packaging is not well controlled, and the temperature is unstable during the processing, which leads to the phenomenon of uneven wall thickness due to uneven heating during the processing. In the processing process, we strengthen the alarm control of each link of the temperature and strictly control the temperature, which helps us reduce the phenomenon of uneven wall thickness caused by the temperature of the tray blister packaging.

   Tray blister packaging wall thickness is not even reason 1: tray blister packaging processing time will also affect the wall thickness of the tray blister packaging, the length of time has a great impact on the temperature and heating time, too long tray blister packaging processing time will lead to the reduction of tray blister packaging accuracy, and too short time, insufficient temperature will also affect the tray blister packaging processing accuracy.

    Tray blister packaging wall thickness is not uniform reason 1: tray blister packaging wall thickness is not uniform and blister process is also affected, if the blister is too deep will also cause tray blister packaging wall thickness is not uniform phenomenon.

Send Message